Abstract

Three hydride-forming mechanical alloys of magnesium with the addition of 10 wt % Ni were synthesized. The mechanical alloys were derived by the method of reactive mechanical alloying (RMA) by different ways, in particular by reactive grinding of Mg powder with Ni additive and by the same reactive grinding under the same conditions of two MgH2 powders made using different methods with the same Ni additives. The effect of this Ni additive and the method of obtaining mechanical alloys (MAs) on the hydrogen sorption properties, temperature and kinetics of decomposition of their MgH2 hydride phase was investigated by isobaric thermodesorption spectroscopy (TDS) at a constant hydrogen pressure of 0.1 MPa. The appreciable influence of the applied method of obtaining MAs on the kinetics of the process of hydrogen desorption is established and the mechanism of the specified influence is investigated.

Files

IISJ_38-22-32.pdf

Files (1.2 MB)

Name Size
md5:b3969ae243da577617c4a5e00359af5e
1.2 MB Preview Download

Additional details

References

  • E.Yu.Ivanov, I.G. Konstanchuk, А.А. Stepanov, Report of the Academy of Sciences 286(2), 385 (1987).
  • G. Liang, J. Huot, S.Вoily, J. Alloys Compd. 292, 247 (1999).
  • J. Huot, G. Liang, R. Schulz, Appl. Phys. A 72, 187 (2001) (DOI: 10.1016/S0925-8388(02)00839-3).
  • R. Attuluri, Vijay Ba, D. Nagaraju, Int. Journal of ChemTech Research.6 (7) 3451 (2016).
  • O.G. Ershova, V.D. Dobrovolsky, Y.M. Solonin, O.Y. Khyzhun, A.Y. Koval. J. Alloys Compd. 464, 212 (2008) (DOI: 10.1016/j.jallcom.2007.10.064).
  • S. Huaiyu, X. Xiubo, J. Li, Nanostructured Mg-Based HydrogenStorage Materials: Synthesis and Properties. Sankir (eds.) (Scrivener Publishing LLC, Hydrogen Storage Technologies, 2018). pp. 89–116.
  • Qun Luo, Jianding Li, Bo Li, Bin Liu, Huaiyu Shao, Qian Li, J. Magnesium and Alloys 7, 58 (2019) (DOI: 10.1016/j.jma.2018.12.001)
  • Sesha Srinivasan, Dervis Emre Demirocak, Ajeet Kaushik, Meenu Sharma, Ganga Ram Chaudhary, Nicoleta Hickman, Appl. Sci. 10, 4618 (2020) (doi:10.3390/app10134618).
  • V. Dobrovolsky, O. Ershova, Yu. Solonin, Innovations in Corrosion and Materials Science 7, 1 (2017) (DOI: 10.2174/2352094907666170607140645).
  • M.Y. Song, Int. J. Hydrogen Energy 20(3), 221 (1995).
  • C.X. Shang, M. Bououdina, Y. Song, Z.X. Guo, Int. J. Hydrogen Energy 29, 73 (2004) (DOI: 10.1016/S0360-3199(03)00045-4).
  • V.D. Dobrovolsky, O.G. Ershova, Yu.M. Solonin, O.Yu. Khyzhun. J.Alloys Comp) 509, 128 (2011) (doi:10.1016/j.jallcom.2010.09.003)
  • Won Ha, Ho-Shin Lee, Jeong-II Youn, Tae-Whan Hong, Young-Jig Kim, Int. J. Hydrogen Energy 3, 1885 (2007) ( doi:10.1016/j.ijhydene.2006.08.029)
  • R.A. Varin, T. Czujko, E.B. Wasmund, Z.S. Wronski, J. Alloys Compd. 446(447), 63 (2007).
  • R.A. Varin, T. Czujko, Z.S. Wronski, Int. J. Hydrogen Energy. 34, 8603 (2009).
  • L Xie, Y. Liu, X. Zhang, Qu, J., Y. Wang, X.Li, J. Alloys Compd. 482, 388 (2009) (doi: 10.1016/j.jallcom.2009.04.028).
  • J. Mao, Z. Guo, X. Yu, H. Liu, Z. Wu, Int. J. Hydrogen Energy 35, 4569 (2010)(doii: 10.3390/en4010001).
  • R. Shahi, P. Tiwari, R. Anand, M.A. Shaz, O.N. Srivastava, Int. J. Hydrogen Energy 38, 2778 (2013) (doi.org/10.1016/j.ijhydene.2012.11.073)
  • H. Yu, S. Bennici, A. Auroux, Int. J. Hydrogen Energy 39, 11633 (2014) (DOI: 10.1016/j.ijhydene.2014.05.069).
  • M. Sherif El-Eskandarany, H.S. AlMatrouk, Ehab Shaban, Ahmed Al-Duweesh, Materials Today: Proceedings 3, 2608 (2016) (www.elsevier.com/locate/procedia)
  • H. Kwak, J.Young, H.Park, R. Song, Y.Myoung, J. Nanoscience and Nanotechnology 17 (11), 8105 (2017) (DOI: 10.1166/jnn.2017.15083)
  • M.S. Yahya, M. Ismail, Int. J. Hydrogen Energy 43, 6244 (2018) (doi.org/10.1016/j.ijhydene2018.02.028)
  • O.G. Ershova, V.D. Dobrovolsky, Yu.M. Solonin, Physics and Chemistry of Solid State 20(4), 406 (2019) (DOI: 10.15330/pcss.20.4.406-415).
  • O.G. Ershova, V.D. Dobrovolsky, Yu.M. Solonin, International independent scientific journal 1(20), 35 (2020).
  • V.D. Dobrovolsky, O.Y. Khyzhun, A.K. Sinelnichenko, O.G. Ershova, Y.M. Solonin, J. Electron Spectroscopy Related Phenom. 215, 28 (2017) (DOI: 10.1016/j.elspec.2017.01.001).
  • V.D. Dobrovolsky, K.I. Kopulova, I.А. Morozov. L.I. Kopulova, Met.Phys.Adv.Tech., 22( 2), 24 (2000)(in Ukrainian).
  • V.D. Dobrovolsky, L.I. Kopylova. Yu.M. Solonin. E.I. Kopylova, Met.Phys.Adv.Tech., 22(11), 32 (2000) (in Ukrainian).
  • V.D. Dobrovolsky, Yu.M. Solonin, E.I. Kopylova, T. V. Khomko. Met.Phys.Adv.Tech. 28(2), 214 (2006) (in Ukrainian).
  • V.D. Dobrovolsky., The correlation between ionicity of metal-hydrogen bonds in hydrides and their thermal firmness. Hydrogen Materials Science and Chemistry of Carbon Nanomaterials. NATO Science Serials.II. Mathematics, Physics and Chemistry, (2007) 421.
  • V.D. Dobrovolsky, O.G. Ershova, Yu.M. Solonin, R.A. Morozova, E.M. Severyanina, J. Alloys Compd. 490, 68 (2010) (DOI:10.1016/j.jallcom.2009.10.105)
  • V.D. Dobrovolsky, O.G. Ershova, Yu.M. Solonin, O.Y. Khyzhun, V. Paul-Boncour, J. Alloys Compd. 465, 177 (2008) (DOI: 10.1016/j.jallcom.2007.10.125).
  • V.D. Dobrovolsky, O.G. Ershova, Ya.M. Solonin, I.Yu. Zavaliy, Carbon Nanomaterials in Clean Energy Hydrogen SystemsII. Springer. (2011) 197.
  • J.F. Stampfer, C.E. Holley, J.F. Suttle, J. Am. Chem. Soc. 82, 3504 (1960) (DOI: 10.1021/ja01499a006).
  • N.Hanada, T. Ichikawa, H. Fujii, J. Phys.Chem. B 109, 7188 (2005)