Published November 1, 2020 | Version v1

Analysis on certain physical and resourceful properties of kish graphite containing materials

Description

Department of Technology Management, the Open University of Kaohsiung, Taiwan

College of Maritime, National Kaohsiung University of Science and Technology, Taiwan

E-mail: edmywu@isu.edu.tw

Manuscript received online 18 November 2020, revised and accepted 30 November 2020

As molten iron flows from furnaces during smelting (the temperature is about 1500°C; the carbon content is between 4.5% ~6.0%), it comes into contact with its surroundings (such as air and fire-resistant elements), causing its temperature to drop to below liquids temperature; at this point, cementite (Fe3C) releases graphite because it is oversaturated. Thanks to its scale-like structure, the released mineral is also known as kish graphite. By using the converter dust from a steel plant in Southern Taiwan, we studied the various physical properties of kish graphite and used a Scanning Electron Microscope (SEM) to observe the properties and structure of its surface.

The result of the sieve analysis indicates that kish graphite took up 5.65% of the composition of the converter dust; in contrast, the result of the elemental analysis shows that the carbon content of the converter dust was 27.99%. From these results, we assume that the low kish graphite content in the converter dust resulted from a drastic temperature drop during the smelting process, which caused a large amount of graphite to disperse into the atmosphere. In terms of the observations on kish graphite through SEM and the Energy Dispersive Spectrometer (EDS), the SEM analysis shows that kish graphite was characterized by a distinct foliated or layered structure and consisted of shattered and loosely distributed graphite. Mean­while, the EDS analysis indicates that kish graphite was not only high in iron oxide, magnesium oxide, zinc oxide and carbon content, but also had a significant amount of impurities attached to its surface. We then assumed that we could remove the different kinds of oxides and minor elements on the surface of the kish graphite by applying liquid acid during the purification process, thus obtaining kish graphite of higher purity. Lastly, after analyzing the degree of weight loss of the converter dust under different temperatures using a thermogravimetric analyzer (TGA), we found that peaks of weight loss at its surface struc­ture appeared between 150~200°C, 350~400°C, 600~700°C, and 700~900°C, with drastic weight reduction being observed under higher temperatures. Consequently, we can state that kish graphite produced from converter dust is characterized by the above-mentioned trends.