Published October 14, 2026
| Version v1
Journal article
Open
Experimental Study on Hybrid Fiber Reinforced Concrete
Description
Concrete is the most widely used construction material in civil engineering practice, valued for its compressive strength, mouldability and durability. Its principal deficiency is mechanical: the material is brittle, its tensile strength is approximately one-tenth of its compressive strength, and once a crack initiates there is little within a plain matrix to arrest its propagation. Hybrid Fiber Reinforced Concrete addresses this by combining fibres of differing geometry and stiffness, so that reinforcement is present at more than one length scale, fine filaments intercepting microcracks at initiation while coarser fibres bridge the macrocracks that form thereafter. This investigation examines M40 grade concrete reinforced with hooked-end steel fibres of aspect ratio 64 and alkali-resistant glass fibres of aspect ratio 857, combined in equal volume fractions at total dosages of 1.0, 2.0 and 3.0 per cent by volume, against a plain control. The mix was proportioned to IS 10262:2019 at a water–cement ratio of 0.40 using Portland Pozzolana Cement. Seventy-two specimens were cast and water-cured. Fresh concrete was assessed by slump and compaction factor; hardened concrete by compressive strength to IS 516, split tensile strength to IS 5816 and flexural strength to IS 516 at 7 and 28 days, supplemented by ultrasonic pulse velocity and rebound hammer testing to IS 13311 upon the same specimens. Every hardened-state property attained its maximum at a total fibre content of 2.0 per cent by volume, comprising 78.5 kg/m³ of steel and 26.8 kg/m³ of glass fibre. Relative to the control, that mix gave improvements of 11.9 per cent in compressive strength, from 46.30 to 51.80 MPa, 30.7 per cent in split tensile strength, from 3.81 to 4.98 MPa, and 30.6 per cent in flexural strength, from 5.42 to 7.08 MPa. The tensile-governed properties therefore improved by between two and three times as much as the compressive strength, which confirms that the benefit arises from crack bridging rather than from densification of the matrix. The ratio of split tensile to compressive strength rose from 0.082 to 0.096, and the measured modulus of rupture exceeded the estimate of Clause 6.2.2 of IS 456:2000 by 14 per cent for the control but by 41 per cent for the optimum mix, showing that fibre reinforcement progressively decouples flexural from compressive capacity. Workability fell sharply, slump reducing by 47.1 per cent across the series and superplasticiser demand rising from 0.80 to 1.30 per cent by mass of cement. The compaction factor fell by only 9.7 per cent over the same range, establishing that slump substantially understates the placeability of fibre reinforced concrete. At the highest dosage the pulse velocity declined together with all three strengths, which identifies incomplete compaction, rather than any deterioration in fibre–matrix interaction, as the cause of the post-optimum reduction. The optimum reported is consequently a property of the compaction procedure as much as of the fibre system. Control specimens failed abruptly whereas fibre reinforced specimens cracked visibly, retained load and remained intact, a change in failure mode of greater practical value than the strength increase itself.
Files
experimental-study-on-hybrid-fiber-reinforced-concrete-IJERTV15IS090960.pdf
Additional details
Related works
- Is identical to
- Journal article: https://www.ijert.org/experimental-study-on-hybrid-fiber-reinforced-concrete (URL)