Published September 18, 2025 | Version v1

Low-temperature heat capacity of modified multiwalled carbon nanotubes with diameter 9.4 nm

  • 1. ROR icon Włodzimierz Trzebiatowski Institute of Low Temperature and Structure Research

Description

The low-temperature specific heat C(T) of multiwalled carbon nanotubes (MWCNTs) with mean outer diameter 9.4 nm, subjected to grinding and grinding-oxidation modifications, was measured from 1.8 K to 275 K. A comparative analysis was performed against initial MWCNTs, bundles of single-walled carbon nanotubes (SWCNT) and graphite. Results indicate that grinding of oxidized MWCNTs increases specific heat relative to initial MWCNTs, maintaining a similar temperature dependence. In contrast, grinding of initial MWCNTs causes different C(T) behavior below 5 K. Above 60 K, the C(T) of all MWCNTs variants, SWCNTs bundles, and graphite converge, reflecting the dominance of 2D graphene sheet phonon density of states. Discrepancies below 60 K are attributed to structural symmetries, potential energies of interaction between walls/sheets/tubes, layer/wall numbers, and defects.

Files

Files (101.3 kB)

Name Size
md5:4025cac2b742453a543ada6781af1ebc
4.4 kB Download
md5:4025cac2b742453a543ada6781af1ebc
4.4 kB Download
md5:3f2d9d3418792ad20e6291743143790f
1.8 kB Download
md5:0aeaee9332c0c419a3646ff97b4eef56
8.8 kB Download
md5:0c8287f9269fb04075f7526dd9ead2a5
8.2 kB Download
md5:bc98069019a271d8fbada99b4c33c66e
8.3 kB Download
md5:f180f66e6bfbd708e83954b79a2262d1
43.0 kB Download
md5:4b07ddee14e4f5b51494ea5d21feaa36
1.7 kB Download
md5:85d7d637dc2ca51b9034e35778fbe4d6
3.7 kB Download
md5:eb1824298993aa362cff37835524e8d8
17.0 kB Download

Additional details

Funding

National Science Centre
2022/45/B/ST3/02326