Published November 23, 2021 | Version v1

Use of bauxite residue as raw material for low-carbon ferrite-belite cements: prediction of the crystalline phases using thermodynamic modelling

Description

In this study, thermodynamic modelling was carried out to predict the crystalline phase and provides a first stepping-stone to incorporate high amounts of BR in low-CO2 cement manufacturing. As raw materials, 35-66 wt% bauxite residue (BR) in combination with 33-64 wt% of limestone (LS) and 1-10 wt% of kaolin (K) were chosen as raw materials for hydraulic low-CO2 ferrite-belite (cement) clinkers. Thermodynamic modelling at a temperature of 1260°C was selected to predict the content of the crystalline phases for the different clinker composition, using the major oxides (i.e., CaO, SiO2, Al2O3, Fe2O3, TiO2 and Na2O). Increasing the BR content (decreasing LS content) led to high amounts of perovskite, gehlenite, iron-rich ferrites, and CaO·Fe2O3 phases. Some of these crystalline phases i.e., perovskite, rankinite and gehlenite are hydraulically inactive; their content is thus aimed to be low. With increasing LS content (decreasing BR content), hydraulic phases such as belites, aluminium-rich ferrite phases, calcium aluminates and free lime dominate the clinker phase assemblage. The highest content of rankinite occurred at a similar LS and BR content of 45-50 wt%. In case of ferrite phases, if the ratio of alumina to iron oxide is equal to or greater than 1, the phases become more hydraulically active in comparison to ratios less than 1. In this study, the ratio of iron oxide to alumina reduces as the LS content is increased from 33-64 wt% and BR content decreased from 66-35 wt%, thus increasing the reactivity of ferrites. Moreover, at a LS content between 55-60 wt% and BR content varying from 35-42 wt%, equal proportions of iron oxide and alumina were obtained for ferrite phases which has positive impact on reactivity. Based on the thermodynamic calculation, the optimum raw mix to develop a favourable low-carbon emission ferrite-belite cement consists of a LS content of 57 wt%, a BR content of 38 wt% and a K content of 5 wt%. This mix design leads to reactive belites and ferrite, of 24 wt% and 63 wt%, respectively, with some minor inactive perovskite phases of about 3 wt%. Overall, this study provides a first stepping-stone to incorporate high amounts of BR in low-CO2 cement manufacturing.

Files

BR08_Prediction_of_the_phase_assemblage_for_low-CO2_emission_ferrite-belite_cements_prepared_using.pdf

Additional details

Funding

European Commission
ReActiv - Industrial Residue Activation for sustainable cement production 958208