A simple cost effective method for obtaining intact shell cenospheres from as received one
Authors/Creators
Description
Department of Chemistry, The Graduate School College for Women, Jamshedpur, Jharkhand, India
E-mail : banashree_h@rediffmail.com
Department of Applied Chemistry, Indian School of Mines, Dhanbad-826 004, Jharkhand, India
Central Institute of Mining and Fuel Research, Dhanbad, Jharkhand, India
Rihand Super Thermal Power Project, Sonebhadra, Uttar Pradesh, India
Manuscript received online 23 May 2013, accepted 28 May 2013
One of the most important value added material found in fly ash are cenospheres. The as received cenospheres collected from an ash lagoon of a super thermal power plant with its size classified fractions were thoroughly characterised. It was revealed that the physical and morphological property differs. Using Scanning Electron Microscopy (SEM) it was found that among the sieved fractions, the coarsest fraction (containing 90–96% by weight of the total as received cenosphere) contains the major fraction of intact shell cenospheres whereas the finest fraction contains mainly the broken one. Further flotation of the coarsest fraction in acetone leads to isolation of a density separated fraction which is lighter and has a higher content of intact shell cenospheres. This floated fraction may act as a better potent for industrial application.