Published September 22, 2021 | Version 08(09)

Evaluation Of Bond Strength Of Splinting Material To The Teeth After Thermocycling - An In Vitro Study

Authors/Creators

  • 1. Senior Lecturer, Department of Periodontics, Saveetha Dental College and Hospitals, Saveetha Institute of Medical and Technical Sciences [SIMATS], Saveetha University

Description

Introduction: Bond strength can be explained, as the amount of adhesion between bonded surfaces. Splints are used to immobilize traumatized teeth that suffered damage in their structures of support, preventing their constant movement. The most frequently used technique is to use orthodontic stainless steel wire, bonded onto the inside surface of the teeth with composite which acts as a splint. Thermocycling is a laboratory method of exposing dental materials and teeth to temperature ranges similar to those occurring in the oral cavity. The aim of this study is to evaluate the bond strength of splinting material to the teeth after thermocycling. Materials and Methods: The experiment consisted of three main steps; namely, preparation of the testing samples, thermocycling and measurement of bond strength. 8 pairs of natural maxillary central incisors were splinted in pairs, using stainless steel orthodontic wire. The 8 pairs were divided in two groups; group 1: where the wire is splinted using bulk filled composite (BFC) and group 2: where the wire is splinted using flowable composite. Both groups were splinted in the same manner. 8 pairs were labelled and wrapped in gauze. Each group was put in the thermocycling machine. After completion of thermocycling, INSTRON E 3000 universal testing machine was used to measure the bond strength, by recording the amount of force it takes to detach the splint from the incisors. After recording the data, and obtaining graphs for the same, the data was analysed using SPSS statistical software. Data analysis was done using an independent sample t test and p value was set as 0.05 as level of significance. Results: In the BFC group, the mean and standard deviation values were 27.5300 and 16.26524. In the flowable composite group, the mean and standard deviation values were 86.2575 and 53.88458. Independent sample t test was done and p value was 0.031 which is less than 0.05, hence statistically significant. Conclusion: Within the limitations of this study, it can be concluded that the splinting of teeth with orthodontic wire using flowable composite shows higher bond strength than bulk filled composite resin after thermocycling.

Files

IJDOS-2377-8075-08-9071.pdf

Files (376.6 kB)

Name Size
md5:21c23bb4b584a94ad4ca2f99a6b99589
376.6 kB Preview Download