Phase Separation in Mixed Compositions Containing Crystallizable Copoly(Uretane-Imide) and Crystallizable Polyimide

Description

A number of samples of copoly(urethane)imides of CPUI (R-TDI-2500-TDI-R)(BAPB)n (n=1,2,3,5) based on poly(diethylene glycol) adipinate (Mn=2500) (2500), bis(3',4-dicarboxyphenoxy)benzene(R dianhydride)and 1,4-bis terminated with 2,4-toluylenediisocyanate (TDI) were synthesized(4'-aminophenoxy)biphenyl (diamine BAPB). CPUI differ in the content of aromatic blocks in the polymer from 37 to 65% (wt of mass). The synthesized samples were characterized by TGA, DSC and MTA methods. CPUI were used to prepare mixed compositions together with polyimide (R-BAPB). The compositions were synthesized in two versions: a) - 10% (wt) and b)-90% (wt), polyimide, respectively. The mixed compositions were investigated using the DSC method. We described the effect of increasing the content of imide links on the values of Tm and Tg copolymers and mixed compositions. This effect is due to the separation and interaction of aromatic (imide) and aliphatic (polyester) phases.

Keywords: copoly(urethane-imide), polyimide, polymer mixture, thermoplastic, thermoplastic, TGA, DSC, MTA, melt rheology, phase separation, rubber-like elasticity.

Files

Phase Separation in Mixed Compositions.pdf

Files (39.6 MB)

Name Size
md5:42580f22efaaaf6b03e744927ff501c5
39.6 MB Preview Download